Need a plan quote or proposal? Available for free 24/7!
Contact: +8619914754015 (WeChat/WhatsApp)
Submit your inquiry for a tailored solution.
{{ variable.name }} : {{ variable.values[selectedVariantsIndex[variable_index]].name }}
Model BF flotation machine is an innovative and upgraded high-efficiency flotation equipment on the basis of Model SF, which is optimized for heavy mineral separation. It adopts unique closed double cut-off cone impeller structure and built-in frothing plate, which generates strong slurry down-circulation and significantly improves the recovery effect of iron ore and other minerals with large specific gravity.BF flotation machine integrates the functions of suction, suction slurry and flotation, and it can be formed into a flotation circuit, which is the ideal choice for the sorting of heavy minerals in the modern mineral processing plant.
Model BF flotation machine realizes high efficiency sorting through the following synergistic process:
Slurry circulation: The unique closed double truncated cone impeller generates strong centrifugal force when rotating at high speed, forming strong slurry down circulation, effectively preventing heavy minerals from precipitation.
Air-slurry mixing: The negative pressure effect of the impeller draws in a large amount of air, which is fully mixed with the circulating slurry and cut into micro-fine bubbles. The built-in bubbling plate further optimizes the size and distribution of bubbles to increase the probability of mineralization.
Mineral Separation: The target mineral particles treated with chemicals collide with the fine air bubbles and attach to them, forming a cluster of mineralized air bubbles. On the premise that the heavy minerals are effectively suspended, the mineralized bubbles steadily rise to the liquid surface, forming an enriched foam layer, which is scraped out by the scraper, thus realizing separation.
Intelligent control: Equipped with automatic control system of the liquid level of the slurry and electric control device, it can realize precise and stable control of the liquid level and the amount of foam scraped out, which is easy to operate.
| Structural design advantages | Performance Advantages |
|---|---|
| Original impeller design: closed double-section cone impeller, light wear and tear, long service life. | High recovery rate: extremely strong suspension ability of heavy minerals, effectively preventing sinking troughs, greatly improving the recovery rate of heavy minerals. |
| Built-in bubbling plate: make air dispersion more uniform, bubble mineralization more fully, high sorting efficiency. | Large processing capacity: powerful slurry and air suction capacity, large processing capacity per unit volume. |
| Modularized design: support horizontal configuration, flexible and convenient process adjustment and capacity expansion. | Lower energy consumption: optimized impeller structure and hydrodynamic design, lower power consumption than similar equipment. |
| Self-priming and self-absorption: no external blower and foam pump are required, and it can form its own flotation circuit with low investment cost. | Stable operation: automatic liquid level control, smooth operation, easy operation and precise adjustment. |
| Easy maintenance: reasonable structural design, key components are easy to replace and maintain. | Strong adaptability: it is especially good at dealing with minerals with high specific gravity and has a wide range of applications. |
| Model | Effective volume (m³) | Impeller diameter (mm) | Impeller circumferential speed (m/s) | Processing capacity (m³/min) | Motor power (kw) | Air intake (m³/m²-min) | Weight of single tank (kg) |
|---|---|---|---|---|---|---|---|
| BF-0.25 | 0.25 | 0.25 | 6.0 | 0.12 - 0.28 | 1.5 | 0.9 - 1.05 | 370 |
| BF-0.37 | 0.37 | 286 | 7.2 | 0.20 - 0.40 | 1.5 | 0.9 - 1.05 | 470 |
| BF-0.65 | 0.65 | 0.65 | 7.35 | 0.30 - 0.70 | 3.0 | 0.9 - 1.10 | 932 |
| BF-1.2 | 1.2 | 1.2 | 7.02 | 0.60 - 1.20 | 5.5 | 0.9 - 1.10 | 1370 |
| BF-2.0 | 2.0 | 2.0 500 | 7.5 | 1.00 - 2.00 | 7.5 | 0.9 - 1.10 | 1750 |
| BF-2.8 | 2.8 | 2.8 550 | 8.06 | 1.40 - 3.00 | 11 | 0.9 - 1.10 | 2130 |
| BF-4.0 | 4.0 | 650 | 8.0 | 2.40 - 4.00 | 4.00 | 0.9 - 1.10 | 2585 |
| BF-6.0 | 6.0 | 6.0 | 7.5 | 3.00 - 6.00 | 18.5 | 0.9 - 1.10 | 3300 |
| BF-8.0 | 8.0 | 760 | 7.5 | 4.00 - 8.00 | 22 | 0.9 - 1.10 | 4130 |
| BF-10 | 10 | 760 | 7.52 | 5.00 - 10.0 | 22 | 0.9 - 1.10 | 4500 |
| BF-16 | 16 | 850 | 8.7 | 8.00 - 16.0 | 37 | 0.9 - 1.10 | 8320 |
| BF-20 | 20 | 850 | 8.7 | 10.0 - 20.0 | 45 | 0.9 - 1.10 | 8670 |
| BF-24 | 24 | 920 | 8.7 | 12.0 - 24.0 | 45 | 0.9 - 1.10 | 8970 |
Note: Please consult the technical engineer for the external dimensions of the equipment (L×W×H). The above parameters are for reference only and may vary due to the nature of materials and process conditions.
Iron ore sorting: Selection and sweeping of magnetite, hematite, etc.
Heavy mineral recovery: ilmenite, chromite, rutile, zircon sand, etc.
Non-ferrous metals: sorting and recovery of tungsten ore, tin ore mud.
Rare metals: tantalum ore, niobium ore and other precious and rare metals selection.
We provide customers with a full range of services to ensure the best performance of the equipment:
Process design support: provide heavy mineral separation scheme optimization and flow design according to your ore characteristics.
Installation and commissioning: send professional engineers to guide the installation and commissioning on site to ensure that the standard and production.
Spare parts supply: Long-term stable supply of original impeller, stator, bushing and other core wear-resistant parts.
Technical training: provide detailed operation and maintenance training for customers.
BF type flotation machine has become the preferred equipment in the field of heavy mineral separation at home and abroad due to its excellent heavy mineral recovery performance, low operating cost and high reliability. Choosing us, you will get not only a piece of equipment, but also a whole set of solutions to improve the efficiency of mineral processing.

To find out more about our products and solutions, please fill out the form below and one of our experts will get back to you shortly.